FADT™ One-Ton Press Capabilities
PUNCHING
The Tamarack Punch Press is capable of quickly punching round holes up to ¼" diameter in any thermoplastic material up to ¼" thick. The chart below contains a list of material thickness limits for punching holes large than ¼".
- The FADT Press can punch round holes up to ¼" diameter in any thermoplastic material up to ¼" thick.
- See the chart for larger hole-punching capabilities.
- Recommend air pressure is 70 PSI for all holes.
Punching Larger Holes |
|||
|
Maximum Material Thickness |
||
Hole Diameter |
Polypropylene |
Co-Poly |
Polyethylene |
¼" or Less |
¼" |
¼" |
¼" |
3/8" |
3/16" |
||
1/2" |
5/32" |
3/16" |
|
RIVETING
Tooling has been developed to form both sides of common rivet shapes and sizes. Copper, aluminum (& some steel) rivets can be formed, as well as setting speedy rivets. Once the rivet is trimmed to the proper length, and the burr is set, the FADT Rivet tooling will shape both the manufactured head and the shop head at once. The chart below contains details on the riveting set-ups.
- For a flat rivet finish, use the SM211 set bit on the PUNCH and/or DIE ADAPTORS. (Speedy Rivets)
- If the combined thickness of materials to be riveted is thin (less than 3/16"), use the 3/8" SPACER (provided) under the DIE ADAPTOR.
- See the chart for the suggested set-ups for forming round rivets heads.
Riveting Set-ups |
|||
Rivet |
Pressure |
Upper Set # |
Lower Buck # |
3/16" Steel |
90 PSI* |
SM291-4704 |
SM200-4558 |
#8 Cu/Al |
80 PSI |
||
#10 Cu/Al |
70 PSI |
SM200-4556 |
|
#12 Cu/Al |
65 PSI |
SM200-4555 |
|
Speedy |
60 PSI |
SM211 |
SM211 |
Sets for "Tubular" style rivets are available – please call! |
|||